| Compressibility | ASTM FA36 | % | 45 |
| Recovery | ASTM FA36 | % | 13 |
| Stress resistance (16h, 300°C) | DIN 52913 | Mpa | 49 |
| Permeability to nitrogen (40bar, RT) | DIN 35356 | mg/(s.m) | <0.02 |
| Ash content of graphite | DIN 51903 | % | <1 |
| Chloride content | FSA NMG 202 | ppm | <50 |
| Fluoride content | FSA NMG 203 | ppm | <50 |
| Density of the graphite | DIN 28090-2 | g/cm3 | 1.0 |
| Compression modulus | DIN 28090-2 | | |
| At room temperature: Eksw | | % | 38 |
| At elavated temperature: Ewsw/300°C | | % | 0.9 |
| Percentage creep relaxation | DIN 28090-2 | | |
| At room temperature: Eksw | | % | 5.0 |
| At elavated temperature: Ewsw/300°C | | % | 4.5 |
| Recovery R | DIN 28090-2 | mm | 0.088 |
| Operating conditions | | | |
| Continuous use max. temperature* | | | |
| Air or oxidizing atmosphere | | °C/°F | 450/842 |
| Reducing or inert atmosphere | | °C/°F | 2500/4532 |
| Continuous use min. temperature* | | °C/°F | -200/-328 |
| Continuous use max. pressure* | | bar/psi | 80/1160 |